First, the edge of the solid wood floor
Lethality: ★★★★☆
The main reason for the warping of solid wood flooring is the dampness of the panel, which directly causes dampness on the solid wood flooring.
(1) The wall and floor of buildings have higher moisture content.
(2) The ground is not completely dry during paving.
(3) The moisture isolation measures are not in place and the water invasion to the floor is not completely blocked.
(4) Including underground pipes, geothermal pipes, condensation water caused by the temperature difference in the room.
(5) The sacrum itself is a completely dry wood.
(6) Artificial water during floor cleaning.
Therefore, we should ensure the drying of the ground and other auxiliary substrates as far as possible before pavement. In particular, moisture isolation measures must be in place. The moisture barrier should ensure the overall seal.
Solution: After finding that the solid wood floor is damp, you should immediately open the floor around the room to dampen the tide. This will ease the deformation. If the damp area is large and the degree of deformation is large, it is recommended that the base be reconstructed and the floor be re-paved after drying.